Acrylic emulsion
Properties
Compared with common cement, it can increase 2-3 times in greatest limit explication percent, 4 times of adhesive strength, 8 times in the the resistance of chlorine ion penetrating power and 1 time of tensive strength and reduce 80% of water adsorption,
Dosage
ash/sand is 0.7-2.5 water/ash is 为 0.2-0.4
polyash ratio is 0.1-0.15( 100kg with 30kgNBS/D.W emulsion )
tirred cement and sand , and add NBS/D.W emulsion, it can be pasted by machine and manual operation.
Uses
used in polymer cement mortar and common cement mortar fow waterworks, port, highway, bridge, metallurgy, chemical industry.
Quality standard
Appearance |
milky white emulsion with slight blue |
Solid |
40±1% |
PH |
2.0-4.0 |
agglomeration limit |
50g/lcn |
Viscosity |
12±0.5S( 4 cup) |
Packing: 200kg per drum or 2.5-25kg per drum
Storage: stored in cool and dry place, ther are no obvious sediment happened in 5-40°C for 3 months
|